Views: 0 Author: MEPER MACHINE Publish Time: 2022-10-13 Origin: MEPER MACHINE
In the production process of MEPER blowing molding machine, there are always various problems, such as the lack of blowing mold, some lack of how we should solve it? Xiaobian is ready for everyone in this article, let's take a look.
I the mold blow molding , how to do
Check the pressure of the hollow blow molding machine in time. The normal air pressure is generally about 2.0-3.0MPA. If the pressure is normal, check whether the exhaust structure of the mold is reasonable, and then adjust the temperature to the appropriate point.
II blow mold shows white , how to do
If the mold is white, the temperature will be reduced and the speed may be added. If the tube does not bake out of the white and blow out of the bottle to white, that is the temperature is low, please add the temperature may decrease the speed.
III how to do the mold thick and thin
This problem is that the bottom of the blow molding product is not in the central position. It can be solved by adjusting the stretch rod to the central position at the bottom of the mold and adding delay blowing.
IV how to do the bottom of the mold after blowing
This situation is mainly because the temperature at the bottom of the bottle is low and the temperature at the mouth of the bottle is high. Please decrease the temperature at the mouth of the bottle and increase the temperature at the bottom of the bottle, and maybe reduce the time of delayed blowing properly.
The above are some common mold blowing problems. I hope the article will be helpful to everyone.